Influence of Waste Glass Powder as a Supplementary Cementitious Material (SCM) on the Mechanical Properties, Expansion, Environmental Impact, and Microstructure of Cementitious Mortar
Bameri, M. ; Mohammadhasani, M. ; Khaloo, A. ; ; NikKhah, M.
Bameri, M.
Mohammadhasani, M.
Khaloo, A.
NikKhah, M.
Publication Date
2025-06-11
End of Embargo
Supervisor
Rights
© 2025 The Authors. Engineering Reports published by John Wiley & Sons. This is an open access article under the terms of the Creative Commons Attribution License, which permits use, distribution and reproduction in any medium, provided the original work is properly cited.
Peer-Reviewed
Open Access status
openAccess
Accepted for publication
Institution
Department
Awarded
Embargo end date
Additional title
Abstract
Incorporating waste glass powder (GP) as a partial replacement for Portland cement (PC) in cementitious mortars offers promising environmental and performance benefits. This study evaluates the effects of varying GP content on setting time, flexural and compressive strength, autoclave expansion, environmental impact, and microstructure. The results indicate that increasing GP content prolongs the setting time due to its lower reactivity compared to PC. Although the early strength of GP-incorporated mortars is substantially lower than that of the control mixture, extended curing durations result in significant strength gains due to ongoing pozzolanic reactions. Autoclave expansion tests show that replacing PC with 30%–40% GP reduces expansion by up to 50%, attributed to the improved particle packing, pozzolanic activity, and optimized pore structure. Environmental impact analysis indicates that both embodied carbon dioxide (ECO2e) and embodied energy (EE) decrease as GP content increases, reflecting its lower environmental footprint compared to PC. Microstructural analysis using scanning electron microscopy (SEM) reveals denser calcium silicate hydrate (C-S-H) crystals and refined pore structures in GP 30% and GP 40% mortars. Additionally, energy-dispersive X-ray spectroscopy (EDX) analysis shows significant consumption of calcium hydroxide (CH) due to the pozzolanic reaction, suggesting reduced risks of alkali-silica reaction (ASR) and sulfate attack, thereby enhancing long-term durability. These findings establish GP as a sustainable supplementary cementitious material (SCM) with significant environmental and performance advantages for future construction applications.
Version
Published version
Citation
Bameri M, Mohammadhasani M, Khaloo A, et al (2025) Influence of Waste Glass Powder as a Supplementary Cementitious Material (SCM) on the Mechanical Properties, Expansion, Environmental Impact, and Microstructure of Cementitious Mortar. Engineering Reports. 7(6): e70238
Link to publisher’s version
Link to published version
Link to Version of Record
Type
Article